Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 115 g/10 min @Load 5.00 kg, Temperature 280 °C |
115 g/10 min @Load 11.0 lb, Temperature 536 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Durethan® DP 1100/30 H2.0 901510 Nylon 6, Micro Glass Balls PA6, molding grade, micro glass balls, good heat-ageing resistance |
|||
Melt Flow | 115 g/10 min @Load 2.16 kg, Temperature 230 °C |
115 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem F1000HC Homopolymer Polypropylene Description: Very High Flexural ModulusApplications: Suggested Uses Include Compounding, Automotive, AppliancesThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.. |
|||
Melt Flow | 115 g/10 min @Load 2.16 kg, Temperature 230 °C |
115 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem TI4900M Impact Copolymer Polypropylene Description: Very high flexural modulus.Applications: Suggested uses include compounding, automotive interior trim, intricately designed parts, thin walled parts.Process: Injection Molding.This resi.. |