Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.200 - 1200 g/10 min | 0.200 - 1200 g/10 min | Average value: 23.4 g/10 min Grade Count:842 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |