Physical Properties Metric English Comments
Melt Flow 13.6 g/10 min

@Load 5.00 kg,
Temperature 280 °C
13.6 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
SABIC Innovative Plastics NORYL GTX GTX675 PPE+PA6
Noryl GTX* GTX675 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to a..
Melt Flow 13.6 g/10 min

@Load 5.00 kg,
Temperature 190 °C
13.6 g/10 min

@Load 11.0 lb,
Temperature 374 °F
Microcell Composite Company CELLAMP® 5100 Pellets
CELLAMP® Pellets can be used for producing foaming boards with damping properties, which yield the best efficiency between -10°C and room temperature.Information provided by Microcell Composite Co..