Physical Properties Metric English Comments
Melt Flow 15.8 g/10 min
15.8 g/10 min
(Condition L) ASTM D-1238
Multibase Multi-Flex® TPE A 6221 NAT
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.