Polymer Property : Melt Flow = 157.2 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 157.2 g/10 min

@Load 5.00 kg,
Temperature 275 °C
157.2 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® B3UG4 BK 23215 20% Glass Filled PA66 FR (Conditioned)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..
Melt Flow 157.2 g/10 min

@Load 5.00 kg,
Temperature 275 °C
157.2 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® B3UG4 BK 23215 20% Glass Filled PA66 FR (Dry)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..
Melt Flow 157.2 g/10 min

@Load 5.00 kg,
Temperature 275 °C
157.2 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Conditioned)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..
Melt Flow 157.2 g/10 min

@Load 5.00 kg,
Temperature 275 °C
157.2 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® C3UG4 20% Glass Filled PA6/66 (Dry)
Description: Halogen-free and phosphorus-free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire ..
Melt Flow 157.2 g/10 min

@Load 5.00 kg,
Temperature 275 °C
157.2 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® C3UG4 20% Glass Filled PA6/66 (Conditioned)
Description: Halogen-free and phosphorus-free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire ..
Melt Flow 157.2 g/10 min

@Load 5.00 kg,
Temperature 275 °C
157.2 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Dry)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..
Melt Flow 157.2 g/10 min

@Load 5.00 kg,
Temperature 275 °C
157.2 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® B3UG4 LS BK 23215 20% Glass Filled PA66 FR (Conditioned)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..
Melt Flow 157.2 g/10 min

@Load 5.00 kg,
Temperature 275 °C
157.2 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® B3UG4 LS BK 23215 20% Glass Filled PA66 FR (Dry)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..
Melt Flow 157.2 g/10 min

@Load 5.00 kg,
Temperature 275 °C
157.2 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® B3UG4 LS Grey 22985 20% Glass Filled PA66 FR (Conditioned)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..
Melt Flow 157.2 g/10 min

@Load 5.00 kg,
Temperature 275 °C
157.2 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® B3UG4 LS Grey22985 20% Glass Filled PA66 FR (Dry)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..