Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 16.2 g/10 min @Load 1.20 kg, Temperature 300 °C |
16.2 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Lehmann & Voss LUVOCOM® 50/CF/30 Polycarbonate, with carbon fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Melt Flow | 16.2 g/10 min | 16.2 g/10 min | |
Kraton® G1652 + PP blend + Talc (12/21/67) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Melt Flow | 16.2 g/10 min @Load 3.80 kg, Temperature 200 °C |
16.2 g/10 min @Load 8.38 lb, Temperature 392 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL V095 PPE+PS (Europe-Africa-Middle East) Noryl* V095 resin is a modified PPE-PS blend that exhibits an excellent balance of non chlorinate, non brominate flame retardance, medium heat/high flow and low specific gravity for light weight par.. |