Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 17.36 g/10 min @Load 5.00 kg, Temperature 300 °C |
17.36 g/10 min @Load 11.0 lb, Temperature 572 °F |
|
Lehmann & Voss LUVOCOM® 1700-7910 PPO, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |