Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 17.6 g/10 min @Load 10.0 kg, Temperature 220 °C |
17.6 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® WR-9120 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 17.6 g/10 min @Load 10.0 kg, Temperature 220 °C |
17.6 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® WR-9120 ASA, Unreinforced Information provided by Samsung Cheil Industries. |