Polymer Property : Melt Flow = 170 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 1.90 - 170 g/10 min
1.90 - 170 g/10 min
Average value: 26.4 g/10 min Grade Count:23
Overview of materials for Nylon 12, Extrusion/Tubing Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values ..
Melt Flow 45.0 - 170 g/10 min
45.0 - 170 g/10 min
Average value: 105 g/10 min Grade Count:6
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum ..