Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 18.1 - 22 g/10 min @Load 1.20 kg, Temperature 300 °C |
18.1 - 22 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Iran Petrochemical (PCC) PC 1822 Polycarbonate Suitable for injection moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Melt Flow | 18.1 g/10 min @Load 2.16 kg, Temperature 300 °C |
18.1 g/10 min @Load 4.76 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP LUBRICOMP DP0039EF PC (Asia Pacific) LNP* Lubricomp* DP0039EF is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated. |
|||
Melt Flow | 18.1 g/10 min | 18.1 g/10 min | Condition S; ASTM D 1238 |
CPT C-Flex® R70-005 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |