Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.500 - 1800 g/10 min | 0.500 - 1800 g/10 min | Average value: 81.3 g/10 min Grade Count:69 |
Overview of materials for Polypropylene, Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Blow Molding Grade". Each property range of values reported is minimum and maximum values.. |