Physical Properties Metric English Comments
Melt Flow 188.38 g/10 min

@Load 5.00 kg,
Temperature 275 °C
188.38 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® C3U BK 23079 PA6/66 FR (Conditioned)
Description: Injection-molding grade with improved flame retardance (free from halogens and phosphorus), used e.g. for impact resistant electrically insulating parts such as contact bases and plug c..