Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 19.9 g/10 min

@Load 5.00 kg,
Temperature 250 °C
19.9 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics NORYL PX1007 PPE+HIPS (Asia Pacific)
PPE/PS, 80degC, FR V-0, high flow