Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.3 g/10 min | 2.3 g/10 min | (Condition L) ASTM D-1238-94a |
Multibase Multi-Pro® 5002 CU Natural 50% Filler Content Polypropylene This product is well suited for non-glossy appliance type parts. It replaces ABS at favorable cost performance characteristics and can be made UV stable. This product can be color matched in most c.. |
|||
Melt Flow | 2.3 g/10 min | 2.3 g/10 min | Condition 230/2-8; ASTM D1238 |
Plaskolite West Optix® CA-81 General Purpose Acrylic Resin Extrusion Grade Pellets. Highest Molecular weight. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® LA-0219-A LDPE Foam Resin Features: Good heat sealing latitudeModerate toughnessEasy processability Applications: Industrial packagingLinersBlends with LLDPEFoam ArticlesInformation provided by Nova Chemicals |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® LA-0219-AM LDPE Foam Resin Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blo.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® LA-0224-A LDPE Foam Resin Excellent stiffness, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blown film.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® LF-0219-D LDPE Film Resin Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Liners, industrial packaging, blends with LLDPE.Data provided by the manufacturer. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® FG220-A Octene LLDPE Film Resin Features: Exceptional toughnessLow gel level Applications: Cast stretch wrapNettingCo-extrusion and laminationInformation provided by Nova Chemicals |
|||
Melt Flow | 2.3 g/10 min | 2.3 g/10 min | ExxonMobil Method |
ExxonMobil LD 503.LN Foams and Compounding Resin
(discontinued **) LD 503.LN is a low density homopolymer specially designed for maximum performance in foam applications.Information provided by ExxonMobil Chemical |
|||
Melt Flow | 2.3 g/10 min | 2.3 g/10 min | Exxon Method |
ExxonMobil Escorene® LD-411 LDPE Power Cable Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable polyethylene homopolymer designed as an electrical grade base resin especially suitable for Henschel blending.Applications: A base r.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) LL0220KJ Linear Low Density Polyethylene LL0220KJ are linear low density polyethylene copolymers containing butane-1 as the comonomer.Applications: shipping sacks, carrier and garbage bags, consumer packaging, high clarity film, agricultu.. |
|||
Melt Flow | 2.3 g/10 min | 2.3 g/10 min | ISO 1133 |
Lucite International Diakon® CRG800 Acrylic Polymer, Toughened Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Melt Flow | 2.3 g/10 min | 2.3 g/10 min | ASTM D1238 |
Lucky IH-830 Acrylic, Injection Grade Similar to grade EH-910, but with higher flow for injection molding. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent.. |
|||
Melt Flow | 2.3 g/10 min | 2.3 g/10 min | |
JPJ Technologies 3000j/JE HDPE Injection Information provided by JPJ Technologies |
|||
Melt Flow | 2.3 g/10 min | 2.3 g/10 min | ISO 1133 |
Lucite International Elvakon® 4461 Medium Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Melt Flow | 2.3 g/10 min @Load 6.60 kg, Temperature 337 °C |
2.3 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM CRS5201 PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Melt Flow | 2.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® MP-0670 ABS, Metal Plating Grade Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 2.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
|
Samsung Cheil Industries Starex® SD-0150GP High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 2.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® MP-0670 ABS, Metal Plating Grade Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 2.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
|
Samsung Cheil Industries Starex® SD-0150GP High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 2.3 g/10 min @Load 2.20 kg |
2.3 g/10 min @Load 4.86 lb |
ASTM D1238 |
Sumitomo Chemical ESPOLEX® WT525 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Melt Flow | 2.3 g/10 min @Temperature 230 °C |
2.3 g/10 min @Temperature 446 °F |
I<sub>2</sub>; ASTM D1238 |
Formosa Plastics Formolene® 3302B Random Copolymer Polypropylene Random Copolymer for Extrusion and Thermoforming Applications Formolene® 3302B is a low melt flow random with excellent clarity, fast cycle time and easy mold release, designed for extrusion proces.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 419.MV Low Density Polyethylene Resin Product Description: LD 419.MV is a LDPE designed for wire and cable applications and is suitable for making crosslinkable compounds for medium voltage insulation.Availability: Latin America, North .. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 503.LP Low Density Polyethylene Resin Product Description: LD 503.LP is a LDPE homopolymer that is suitable for use in molding, extrusion, compounding and foam applications.Availability: Latin America, North America and South AmericaAdd.. |
|||
Melt Flow | 2.3 g/10 min | 2.3 g/10 min | ASTM D1238 |
Dow DOWLEX™ 2047G Linear Low Density Polyethylene For high performance stretch film applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem FL31 LLDPE Cast Film Extrusion Polyethylene Copolymer FL31 is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process. It was developed for cast film extrusion. Films obtained with this product show a good processing .. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 235 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AESN P20 TL Nylon 12, Flexible Grade (Dry) Designation ISO 1874-PA12-P,EHL,22-005Flexible grade for overmolding. Available colors: natural and white. Light and heat stabilized. No lubricant.Flexibility. Very good ability to overmold Pebax an.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem LH218 Linear Low Density Polyethylene Insulation for low and medium tension XLPE wires and cables.Information provided by Braskem. |
|||
Melt Flow | 2.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Americas Styrenics STYRON® 404 High Impact Polystyrene Product CharacteristicsAdditive FreeTypical ApplicationsCompounding and masterbatchesInformation provided by AmericasStyrenics LLC. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 235 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AZM 43 G9 T6LD Nylon 12, 43% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLS,16-080,(G+C)(F+D)(43+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
Melt Flow | 2.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 300ATB BK000 Acetal Homopolymer
(Unverified Data**) Delrin® 300ATB BK000 is a filled, medium viscosity, toughened acetal homopolymer for injection molding. It is well suited for antistatic applications.Information provided by DuPont Performance Poly.. |