Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.40 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.40 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1000-95 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 2.40 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ExxonMobil Method |
ExxonMobil HD 7925.30 Barrier Film Resin Product Description: HD 7925.30 is a medium molecular weight HDPE homopolymer for use in blown and cast film applications. Typical applications include those with low WVTR and clarity requirements.A.. |