Melt Flow 2.63 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.63 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Arkema Group Evatane® 1020 VB 2 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for transparent, resistant films, sealable at low temperature. Examples: laminates.ISO data provided by the manufacturer, Arke..
Melt Flow 2.63 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.63 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Arkema Group Evatane® 1020 VB 3 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for molding rigid articles. Examples: closures, ice trays.ISO data provided by the manufacturer, Arkema.
Melt Flow 2.63 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.63 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Arkema Group Evatane® 1020 VG 2 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for resistant films, sealable at low temperature with some hot tack. Examples: bags, deep-freeze packaging, laminates, coextru..