Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 20.8 g/10 min @Load 2.16 kg, Temperature 260 °C |
20.8 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® SLDM310 PC (Asia Pacific) Mineral filled Antistatic Polycarbonate, HDT110degC type |
|||
Melt Flow | 20.8 g/10 min @Load 10.0 kg, Temperature 250 °C |
20.8 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL N1052P PPE+HIPS (Asia Pacific) PPE+PS 105deg.C FR V-2 |