Polymer Property : Melt Flow = 21.7 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 21.7 g/10 min

@Load 5.00 kg,
Temperature 345 °C
21.7 g/10 min

@Load 11.0 lb,
Temperature 653 °F
Lehmann & Voss LUVOCOM® 1100-8401 Polyether sulfone, unreinforced
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Melt Flow 21.7 g/10 min

@Load 5.00 kg,
Temperature 190 °C
21.7 g/10 min

@Load 11.0 lb,
Temperature 374 °F
Microcell Composite Company CELLAMP® 5000 Pellets
CELLAMP® Pellets can be used for producing foaming boards with damping properties, which yield the best efficiency between -10°C and room temperature.Information provided by Microcell Composit..