Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 22.8 g/10 min @Load 5.00 kg, Temperature 200 °C |
22.8 g/10 min @Load 11.0 lb, Temperature 392 °F |
|
Microcell Composite Company CELLOMER® 6000 SBS Rubber Pellets CELLOMER® PELLETS can be used in hot-pressing or with injection foaming boards. Featuring anti-slippage and elasticity.Information provided by Microcell Composite Company |
|||
Melt Flow | 22.8 g/10 min @Load 5.00 kg, Temperature 250 °C |
22.8 g/10 min @Load 11.0 lb, Temperature 482 °F |
|
Lehmann & Voss LUVOCOM® 1850-7581-1 PBT, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |