Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 23.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
23.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1791R4 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 23.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
23.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron IPM3000 PMMA- ABS Alloy Super High Gloss, High scratch resistanceInformation provided by Bhansali |
|||
Melt Flow | 23.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
23.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron IPM3000 PMMA- ABS Alloy Super High Gloss, High scratch resistanceInformation provided by Bhansali |