Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 27.5 - 95.1 g/10 min | 27.5 - 95.1 g/10 min | Average value: 50.8 g/10 min Grade Count:6 |
Overview of materials for Nylon 11, Cable Sheathing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Cable Sheathing Grade". Each property range of values reported is minimum and maximum values o.. |
|||
Melt Flow | 27.5 g/10 min @Load 2.16 kg, Temperature 250 °C |
27.5 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® FXV310SK PBT VALOX FXV310SK is an unreinforced PBT injection moulding Visualfx* resin with high flow characteristics and containing a metal sparkle. Applications: automotive bezels and appliances. |
|||
Melt Flow | 27.5 g/10 min @Load 2.16 kg, Temperature 235 °C |
27.5 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® BECN W3 TL Nylon 11, Sheathing Grade (Conditioned) Designation ISO 1874-PA11,KFHL,12-010Rigid grade for sheathing wires and cables. Available color: natural. Light and heat stabilized. Flame retardant agent.Fire-resistant. High abrasion resistance. .. |
|||
Melt Flow | 27.5 g/10 min @Load 2.16 kg, Temperature 235 °C |
27.5 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® BECN W3 TL Nylon 11, Sheathing Grade (Dry) Designation ISO 1874-PA11,KFHL,12-010Rigid grade for sheathing wires and cables. Available color: natural. Light and heat stabilized. Flame retardant agent.Fire-resistant. High abrasion resistance. .. |