Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 29.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
29.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
S&E Specialty Polymers TufFill™ 5003UV Polyolefin Application: Thermoplastic polyolefin material is designed for molded in color automotive interior and exterior application. This product can be supplied in natural or an OEM matched color with UV p.. |