Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 29.44 g/10 min @Load 10.0 kg, Temperature 380 °C |
29.44 g/10 min @Load 22.0 lb, Temperature 716 °F |
|
Lehmann & Voss LUVOCOM® 1105/BK7308 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Not f.. |
|||
Melt Flow | 29.44 g/10 min @Load 10.0 kg, Temperature 380 °C |
29.44 g/10 min @Load 22.0 lb, Temperature 716 °F |
|
Lehmann & Voss LUVOCOM® 1105/BK7308-1 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Not f.. |