Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 29.7 g/10 min @Load 5.00 kg, Temperature 300 °C |
29.7 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PX1340 PPE+HIPS (Asia Pacific) PPE+PS MF Filled |