Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.92 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.92 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Arkema Group Evatane® 1020 VG 3 Ethylene Vinyl Acetate EVA copolymer made by high process tubular process. Applications Grade for transparent films, high strength, sealing at low temperature, hot tack. Examples: laminates, coextrusion, secondary sealing.. |
|||
Melt Flow | 3.92 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.92 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Arkema Group Evatane® 1020 VN 3 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for flexible, very transparent films with high strength, very good sealability. Examples: thin stretch film for food packaging.. |