Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.96 - 91.0 g/10 min | 3.96 - 91.0 g/10 min | Average value: 32.0 g/10 min Grade Count:6 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |
|||
Melt Flow | 3.96 - 13.2 g/10 min @Load 2.16 kg, Temperature 400 °C |
3.96 - 13.2 g/10 min @Load 4.76 lb, Temperature 752 °F |
ASTM D1183 |
Gharda Chemicals GATONE™ 5300 PEEK, High Viscosity Grade
(discontinued **) High viscosity grade for extrusion and injection moldingCHARACTERISTICS: Outstanding chemical resistance.Outstanding wear resistance.Outstanding resistance to hydrolysis.Excellent mechanical propert.. |