Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 30 - 33 g/10 min @Load 2.16 kg, Temperature 230 °C |
30 - 33 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Samyang Triel® 5302FR Thermoplastics Polyetherester Elastomer, Non-Halogen Flame Retardancy Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5302FR is a non-halogen, flame retardant grade.Information provided by Samyang. |