Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.00 - 37.0 g/10 min | 1.00 - 37.0 g/10 min | Average value: 14.0 g/10 min Grade Count:9 |
Overview of materials for Polyphenylene Ether, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ.. |
|||
Melt Flow | 1.00 - 37.0 g/10 min | 1.00 - 37.0 g/10 min | Average value: 12.9 g/10 min Grade Count:34 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Melt Flow | 1.21 - 37.0 g/10 min | 1.21 - 37.0 g/10 min | Average value: 10.9 g/10 min Grade Count:31 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Melt Flow | 0.800 - 37.0 g/10 min | 0.800 - 37.0 g/10 min | Average value: 10.6 g/10 min Grade Count:8 |
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu.. |
|||
Melt Flow | 2.00 - 37.0 g/10 min | 2.00 - 37.0 g/10 min | Average value: 21.2 g/10 min Grade Count:5 |
Overview of materials for Silicone Polyurethane, Ether Based This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum value.. |