Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.00 - 38.8 g/10 min | 1.00 - 38.8 g/10 min | Average value: 16.8 g/10 min Grade Count:14 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |