Melt Flow 39.6 - 52.8 g/10 min

@Load 2.16 kg,
Temperature 400 °C
39.6 - 52.8 g/10 min

@Load 4.76 lb,
Temperature 752 °F
ASTM D1183
Gharda Chemicals GATONE™ 5600 PEEK, Low Viscosity Grade  (discontinued **)
Low viscosity. grade for injection molding of thin sections & complex partsCHARACTERISTICS: Outstanding chemical resistance.Outstanding wear resistance.Outstanding resistance to hydrolysis.Excellen..