Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 4.4 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 4.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Eastman M3006-P Polyethylene  (discontinued **)
Medium density polyethylene M3006-P is a specialty formulation suggested for high speed extrusion coating applications. M3006-P offers improvements over low density polyethylene in barrier properti..
Melt Flow 4.4 g/10 min

@Load 10.0 kg,
Temperature 220 °C
4.4 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
LG Chemical BM662 ABS, Heat Resistance
Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical..
Melt Flow 4.4 g/10 min

@Load 3.80 kg,
Temperature 230 °C
4.4 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM-D1238
Ineos ABS Lustran® 451 ABS, Injection Molding Grade
Lustran® ABS 451 is a soft flowing, medium impact injection molding resin designed with a unique balance of impact, heat resistance, flow, and gloss.
Melt Flow 4.4 g/10 min
4.4 g/10 min
ISO 1133
Lucite International Diakon® CMG302 Acrylic Polymer
Information provided by Lucite International
Melt Flow 4.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Techmer ES HiFill® HDPE 8904 UV GY
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceAppearance: GreyInformation provided by TP Composites, Inc.
Melt Flow 4.4 g/10 min

@Load 2.20 kg
4.4 g/10 min

@Load 4.86 lb
ASTM D1238
Sumitomo Chemical ESPOLEX® WT487X Thermoplastic Elastomer
ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi..
Melt Flow 4.4 g/10 min

@Load 5.00 kg,
Temperature 230 °C
4.4 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Chi Mei Polylac® PA-747S ABS - Extrusion
High Impact Extrusion
Melt Flow 4.4 g/10 min

@Load 5.00 kg,
Temperature 200 °C
4.4 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ASA M-143
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
Melt Flow 4.4 g/10 min
4.4 g/10 min
ASTM D1238
Huntsman Rexell® L3103 Blown Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Excellent optics and sealability with good toughnessApplications: Stretch wrap and coextruded film for general packaging.FD..
Melt Flow 4.4 g/10 min
4.4 g/10 min
ASTM D1238
Huntsman Rexell® M3107 Blown Film Extrusion LLDPE  (discontinued **)
Linear-low medium density copolymer, cast film extrusion, FDA compliantFeatures: Excellent combination of stiffness, heat resistance, and impermeability to water vapor.Applications: Food packaging, ..
Melt Flow 4.4 g/10 min
4.4 g/10 min
ASTM D1238
Huntsman Rexell® V3101 Blown Film Extrusion LLDPE  (discontinued **)
Linear-low very low density copolymer, cast film extrusion, FDA compliant.Features: High toughness, puncture resistance with good sealing and excellent optical properties.Applications: Food packagin..
Melt Flow 4.4 g/10 min
4.4 g/10 min
ISO 1133
Lucite International Diakon® MG102 Acrylic Bead Polymer, High Transparency
PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte..