Melt Flow 41.7 g/10 min

@Load 2.16 kg,
Temperature 275 °C
41.7 g/10 min

@Load 4.76 lb,
Temperature 527 °F
ISO 1133
BASF Ultradur® S 4090 G4X 20% Glass Filled PBT
Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 20% of glass fibers for industrial parts with high dimensional stab..