Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 42.24 g/10 min @Load 10.0 kg, Temperature 380 °C |
42.24 g/10 min @Load 22.0 lb, Temperature 716 °F |
|
Lehmann & Voss LUVOCOM® 1105/BK0873 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Especially suitable for medical parts, super.. |