Melt Flow 45.9 g/10 min

@Load 1.20 kg,
Temperature 300 °C
45.9 g/10 min

@Load 2.65 lb,
Temperature 572 °F
Lehmann & Voss LUVOCOM® 19-7816 Polyamide 46, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrical..