Polymer Property : Melt Flow = 47 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 47 g/10 min

@Load 2.16 kg,
Temperature 230 °C
47 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Ineos H44N-00 Polypropylene Homopolymer
H44N-00 is a high flow rate, nucleated polypropylene homopolymer designed for compounding and injection molding applications. The grade benefits from a high stiffness and isotropic shrinkage to help..
Melt Flow 47 g/10 min

@Load 2.16 kg,
Temperature 190 °C
47 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Ineos T50-4400 HDPE
Ineos T50-4400 is a high-flow high density polyethylene copolymer intended for injection molding of thin wall containers. This material will allow for cycle time reduction while still imparting rea..
Melt Flow 47 g/10 min

@Load 5.00 kg,
Temperature 266 °C
47 g/10 min

@Load 11.0 lb,
Temperature 511 °F
ASTM D1238
SABIC Innovative Plastics LNP STAT-KON Valox_VCF2020 PET
LNP* Stat-kon* Valox_VCF2020 compound is a 20% carbon fiber reinforced PET. Conductive applications.
Melt Flow 47 g/10 min

@Load 10.0 kg,
Temperature 250 °C
47 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Melt Flow 47 g/10 min

@Load 10.0 kg,
Temperature 250 °C
47 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Samsung Cheil Industries Infino® WP-1069 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Melt Flow 47 g/10 min

@Load 2.16 kg,
Temperature 230 °C
47 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238L
Braskem CP 141 Injection Molding Polypropylene
Description: CP 141 is a high melt flow rate heterophasic copolymer specially designed to achieve high productivity on thin-walled parts with very easy mould filling and high speed injection mouldin..