Polymer Property : Melt Flow = 5.20 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 5.20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil LLP8360.29 Rotational Molding Resin
Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui..