Physical Properties Metric English Comments
Melt Flow 50.05 g/10 min

@Load 5.00 kg,
Temperature 250 °C
50.05 g/10 min

@Load 11.0 lb,
Temperature 482 °F
Lehmann & Voss LUVOCOM® 1850/CF/15/TF/10/EM PBT, with carbon fiber, PTFE, easy flowing
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita..