Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 56.8 g/10 min @Load 10.0 kg, Temperature 380 °C |
56.8 g/10 min @Load 22.0 lb, Temperature 716 °F |
|
Lehmann & Voss LUVOCOM® 1105-8160 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |