Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 69.4 g/10 min @Load 2.16 kg, Temperature 235 °C |
69.4 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AMN D Nylon 12, Rigid, Injection Grade (Dry) Designation ISO 1874-PA12,MR,14-010Rigid grade for injection molding. Available colors: black, natural, orange, red and white. Possibilities of heat and light stabilizing agents. mold-release agent... |
|||
Melt Flow | 69.4 g/10 min @Load 2.16 kg, Temperature 235 °C |
69.4 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AMN D Nylon 12, Rigid, Injection Grade (Conditioned) Designation ISO 1874-PA12,MR,14-010Rigid grade for injection molding. Available colors: black, natural, orange, red and white. Possibilities of heat and light stabilizing agents. Mold-release agent... |