Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 40 - 70 g/10 min | 40 - 70 g/10 min | Melt Volume Rate (cm³/10 min) |
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Melt Flow | 59.1 - 70 g/10 min @Load 1.20 kg, Temperature 300 °C |
59.1 - 70 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Iran Petrochemical (PCC) PC 5970 Polycarbonate Suitable for injection moldingInformation provided by Iran Petrochemical Commercial Co. |