Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 70.8 g/10 min @Load 2.16 kg, Temperature 235 °C |
70.8 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AUM 30 T6LD Nylon 12, 30% Glass Bead Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-020,GB30Rigid grad with glass beads filler (30%) for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Reinforce.. |
|||
Melt Flow | 70.8 g/10 min @Load 2.16 kg, Temperature 235 °C |
70.8 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AUM 30 T6LD Nylon 12, 30% Glass Bead Filled (Dry) Designation ISO 1874-PA12,MHLR,16-020,GB30Rigid grad with glass beads filler (30%) for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Reinforce.. |