Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 62 - 72 g/10 min @Load 2.16 kg, Temperature 235 °C |
62 - 72 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238 |
Gromax PBT 1200-211D Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle.. |