Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 60 - 75 g/10 min | 60 - 75 g/10 min | ISO 1133 |
Beijing Ranger Chem BLUESTAR® 1079 PBT Can be used directly for spinning, and producing color concentrates. It can also be used for production after reinforcement & compounding.Information provided by Beijing Ranger Chemical Co. |