Physical Properties Metric English Comments
Melt Flow 750 g/10 min

@Load 5.00 kg,
Temperature 316 °C
750 g/10 min

@Load 11.0 lb,
Temperature 600 °F
ASTM D1283
Chevron Phillips Ryton® PR26 Polyphenylene Sulfide Resin  (discontinued **)