Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 78.65 g/10 min @Load 5.00 kg, Temperature 275 °C |
78.65 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 527 |
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Conditioned) Ultramid B3G8 BK00564 is a 40% glass filled, pigmented black, injection molding PA6 grade. |
|||
Melt Flow | 78.65 g/10 min @Load 5.00 kg, Temperature 275 °C |
78.65 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Dry) Ultramid B3G8 BK00564 is a 40% glass filled, pigmented black, injection molding PA6 grade. |