Polymer Property : Melt Flow = 8.15 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 8.15 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.15 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Noble Polymers Ecobarrier™ 2412 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..