Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 8.56 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.56 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Luran® S 757 R Colored ASA Description: General-purpose grade for injection molding with high stiffness.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |