Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 8.82 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.82 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Lehmann & Voss LUVOCOM® 80-7489 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |