Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 81 g/10 min @Load 2.16 kg, Temperature 190 °C |
81 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 2717 HDPE Injection Molding Resin
(discontinued **) Features: Super high flow, good balance of toughness and stiffness, low odor, permits container weight reduction.Applications: Thin walled food containers.Data provided by the manufacturer. |
|||
Melt Flow | 81 g/10 min @Load 5.00 kg, Temperature 266 °C |
81 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 855 PBT 15% GR PBTP, UL94 V-0 rated. Improved surface appearance. For external housings: steam irons, appliance housings and lighting parts. |
|||
Melt Flow | 81 g/10 min @Load 5.00 kg, Temperature 266 °C |
81 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 855 PBT (Asia Pacific) 15% GR PBTP, UL94 V-0 rated. Improved surface appearance. For external housings: steam irons, appliance housings and lighting parts. |