Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 9.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Silon TA 2347 HD Orange Catalyst Masterbatch Masterbatch for use with SILON Silane cross-linkable PE-Xb Compounds TA 1108 HD.TA 2347 HD, together with the above mentioned graft, contains the cross-linking catalyst to complete a Sioplas System... |